The treated fluoropolymer film and rubber are adhered using vulcanized adhesion and then the 180° peeling strength test is conducted. The result shows that the average peeling strength of 12.6 N/mm is ...
MA-g-EPDM coated EPDM and FKM (previously mixed) blends were prepared on laboratory size two-roll mixing mill and the temperature maintained at 70 ± 5 ºC. The duration of the mixing time is 20 minutes ...